aterial bone | 45# steel |
Spary material: | Tungsten Carbide(wolfram carbide) |
Surface roughness | Ra 0.3 |
Thickness of Coating: | 2-3 mm single side |
Hardness of Coating: | HRC 65 |
Craft: | Melting after coating to ensure the coating powder and the base metallurgical connection. |
Coating feature: | wearing-proof, fit for making cooper wire,
stainless wire with Φ 0.5mm and above. |
equippment | Supersonic equipment(HVOF),flame powder spray equipment |
Typical coat(Tungsten carbide ): | CO-WC coat,self-fusion alloy+(30-50)%WC coat |
Drawing | Customs provide technical drawing or finish with us |
Certification | ISO9001 |
Sample Lead time | From 5 days to 7 days upon receipt of sample charge |
Delivery Lead time | 10-15 days after deposit received |